Mold flow assist to design Laser printer mold design and plastic injection processing
DengFeng mold had designed so many kinds of Motormeter mold construction such as Honda, VW, TOYOTA etc.. We are good at this kinds of field.
Detaisl contact: Jacky Qiu: 8613533665622
Skype: df mold
One-stop plastic injection molding Details: Jacky Qiu MSN: dfmold@yahoo.com Differential Shrinkage
This type of shrinkage is often caused by variation in crystalline content and volumetric shrinkage. The following figure shows a thin rib attached to a thick top. In general, the cooling rate of the top will be lower than that of the thin section. The top will have increased crystalline content and therefore, will shrink more and cause the warpage shown.
The following figure (a) shows saddle warping of a centrally gated disk with high shrinkage around the gate. Conversely, if the shrinkage is higher around the outer part of the disk, the resulting warpage may cause the disk to dome, shown in (b).
Differential Cooling
Shrinkage due to differential temperature typically results in bowing of the component, as shown in the figure below. Usually this type of shrinkage is due to poor cooling system design.
While the part is in the mold, temperature differences from one side of the mold to the other cause variations in shrinkage through the thickness of the component. In addition to this, any temperature differences at ejection will cause further warpage as both sides of the part cool to room temperature.
Specification: |
|
Certificates |
AAA grade credit enterprise, ISO9001, ISO14001, SGS |
Quality-guaranteed |
Japanese standard of QC management & Euramerican standards |
Service |
Designing the mould, CNC processing and other tooling, assemble all mould parts |
OEM & ODM service |
Acceptable |
Design software |
UG, PRO-E, CAD, CAXA, etc |
Mould base Standard |
LKM , HASCO , DME, etc |
Moulds’ steel |
NAK80, S136(H), 2738, 718&738 and P20 etc |
hardness of steel: |
15--60 HRC |
cav/core material |
2738,2343,DIN-1,S130,2344,738H,718,8407,S136,NAK80,P20 etc |
Cavity |
Single/multi |
Runner |
Hot/cold |
Mould life |
500,000-1,000,000 shots as you required |
Final products’ materials |
ABS, PP, PE, POM, PA6(66)+GF, PC, PMMA HIPS, GPPS etc |
Final Products’ colors |
Any color as your required |
Lead Time |
25-50 workdays based on the different products |
Relevant requirements reachable |
ROHS, UL, or as requested |
Package |
Wooden case package or follow customers' requirement |
Price Terms |
FOB Shanghai Port, China |
Payment term |
T/T, L/C at sight |
Details contact: Jacky Qiu Skype: df mold